Polymer Property : Tensile Modulus = 84.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.580 GPa
84.1 ksi
cond; ISO 527-1/-2
DSM Novamid® ST220 NAT PA6-I
Impact Modified, Injection Molding, Medium Viscosity
Tensile Modulus 0.580 GPa
84.1 ksi
1 mm/min
Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EFHL,22-003Flexible grade for tubes extrusion. Available color: milky white. Light and heat stabilized. Flame retardant agent.Fire-resistant. Flexibility. High impact str..