Mechanical Properties Metric English Comments
Tensile Modulus 5.79 GPa
840 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2212EPR PEI
20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising.
Tensile Modulus 5.79 GPa
840 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific)
20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising.
Tensile Modulus 5.79 GPa
840 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6
LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 5.79 GPa
840 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp TX88477 PU
LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 5.79 GPa

@Temperature 175 °C
840 ksi

@Temperature 347 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry  (discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..