Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.08 GPa | 882 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber. |
|||
Tensile Modulus | 6.08 GPa | 882 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers. |
|||
Tensile Modulus | 6.08 GPa | 882 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber. |