Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.12 GPa | 1320 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 9.12 GPa | 1320 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Tensile Modulus | 9.12 GPa | 1320 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SU PP LNP* THERMOCOMP* MF006SU is a compound based on Polypropylene containing 30% lass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized. |