Mechanical Properties Metric English Comments
Tensile Modulus 0.0660 GPa
9.57 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..