Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.84 GPa | 1430 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp WX01910L PBT LNP* Thermocomp* WX01910L is a compound based on Thermoplastic Polyester containing Proprietary Fillers. Characteristics of this grade are: Low Extractable.This data was supplied by SABIC-IP for t.. |
|||
Tensile Modulus | 9.84 GPa | 1430 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Tensile Modulus | 9.84 GPa | 1430 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare. |