Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.96 GPa | 1440 ksi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PI-30GF/000R BLACK Polyether Imide (PEI) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 9.96 GPa | 1440 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36 PA6.12 LNP LUBRICOMP* IFL36 is a compound based on Nylon 6/12 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 9.96 GPa | 1440 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP REL22 PA 66 LNP* LUBRICOMP* REL22 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Electrically Conductive. |