Polymer Property : Tensile Modulus = 906.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.248 GPa
906.2 ksi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
CRP Technology Windform® LX 2.0 Polyamide Composite
Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability ..