Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 35.0 N @Thickness 0.00300 mm |
7.87 lb (f) @Thickness 0.000118 in |
perpendicular; ISO 34C |
Total PS CPDS 9217 Compound Polystyrene/Polyethylene POLYSTYRENE (PS) COMPOUND (CPDS) 9217 is an alloy of polystyrene and polyethylene. This combination brings the benefits of polyethylene; a high level of stress crack resistance, mechanical properti.. |