Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 1.05 MPa-m½ | 0.956 ksi-in½ | |
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |