Polymer Property : Fracture Toughness = 0.967 MPa-m½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 0.967 MPa-m½
0.880 ksi-in½
Hexcel® HexPly® M65 Bismaleimide Resin
HexPly® M65 is a bismaleimide resin that cures via an addition reaction in a toughened two-phase thermoset matrix with no condensation by-products. HexPly® M65 is a controlled flow polyimide resin..