Polymer Property : Fracture Toughness = 103 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 113 MPa-m½

@Treatment Temp. 496 °C
103 ksi-in½

@Treatment Temp. 925 °F
496°C Temper Temperature, TL Orientation, Core; ASTM E399
Latrobe CSS-42Lâ„¢ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel
CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness ..