Mechanical Properties Metric English Comments
Fracture Toughness 120 MPa-m½
109 ksi-in½
K<sub>e</sub>; T-L; &#916;a<sub>e</sub> = 20 mm
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy
Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f..
Fracture Toughness 120 MPa-m½
109 ksi-in½
K<sub>e</sub>; L-T; &#916;a<sub>e</sub> = 20 mm
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy
Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f..