Polymer Property : Fracture Toughness = 13.7 MPa-m½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 13.7 MPa-m½
12.5 ksi-in½
Average K<sub>IC</sub>.
Materion E20 Beryllium/BeO Composite, 20 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..