Polymer Property : Fracture Toughness = 16.482 MPa-m½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 16.482 MPa-m½
15.000 ksi-in½
T-L
Kaiser 7068 T6, T6511 Rod & Bar
Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig..