Fracture Toughness 165 MPa-m½
150 ksi-in½
K(Q)
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties
Data provided by Carpenter Technology Corporation.This is a carburizing, corrosion resistant steel designed to provide a case hardness in excess of HRC 60 combined with a tough, ductile core. The c..
Fracture Toughness 165 MPa-m½
150 ksi-in½
Latrobe Lescalloy® AF 1410 VIM-VAR ; 6 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..