Polymer Property : Fracture Toughness = 2.82 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 3.10 MPa-m½
2.82 ksi-in½
Ceradyne CeraTrex™ SC-P2 Silicon Carbide
Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company
Fracture Toughness 3.10 MPa-m½
2.82 ksi-in½
Ceradyne CeraTrex™ SC-P3 Silicon Carbide
Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company