Mechanical Properties Metric English Comments
Fracture Toughness 29.0 - 32.0 MPa-m½
26.4 - 29.1 ksi-in½
tempering range 200-450°C (390-842°F) respectively. Hardened at 960°C (1760°F). Quenched in air. Tempered twice.
Assab Steels CALMAX Plastic Mold Material
CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo..