Polymer Property : Fracture Toughness = 3.82 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 4.20 MPa-m½
3.82 ksi-in½
K<sub>IC</sub>
CeramTec Rubalit® A 1894 Alumina, 94%
Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..
Fracture Toughness 4.20 MPa-m½
3.82 ksi-in½
DIN 51109
CeramTec 433 Alumina, 99.9%
433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A ..
Fracture Toughness 4.20 MPa-m½
3.82 ksi-in½
K<sub>IC</sub> (SEVNB); DIN CEN/TS 14425-1
CeramTec B 40 Alumina, 99.1%
B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability.