Polymer Property : Fracture Toughness = 41.0 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness >= 45.0 MPa-m½
>= 41.0 ksi-in½
K(IC)
TIMET TIMETAL® 834 (Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35Si-0.06C) Titanium Alloy
High-Strength, High Temperature, Creep Resistant AlloyIndustry Specifications: France: T-A6EZ r4Nb.Features: TIMETAL 834 is a near alpha titanium alloy offering increased tensile strength and creep..