Polymer Property : Fracture Toughness = 5.60 MPa-m½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 5.60 - 6.80 MPa-m½
5.10 - 6.19 ksi-in½
China-Yixing Longly Refractories Alumina Grinding Balls and Lining Bricks Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks
Characteristics: LONGLY adopts isostatic pressing and dry pressing in the forming process. We provide a variety of products with different dimension and specification. These products are extremely..