Fracture Toughness 65.0 - 69.0 MPa-m½
59.2 - 62.8 ksi-in½
K(IC); Typical Bar (heat treatment unspecified); Longitudinal
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated
High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL..
Fracture Toughness 65.0 - 69.0 MPa-m½
59.2 - 62.8 ksi-in½
K(IC); Typical Bar (heat treatment unspecified); Longitudinal
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged
High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL..