Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.000296 GPa @Strain <=25.0 % |
0.0430 ksi @Strain <=25.0 % |
ASTM D1002 |
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb.. |
|||
Shear Modulus | 0.000296 GPa | 0.0430 ksi | ASTM D1002 |
Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring.. |