Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.000331 GPa | 0.0480 ksi | ASTM D 1002 |
Arlon R36601A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Sty.. |