Polymer Property : Shear Modulus = 0.000410 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.000410 GPa

@Strain 100 %
0.0595 ksi

@Strain 100 %
NF T 46-023
SMAC SMACTANE® SP Damping Material
A viscoelastic rubber material developed by SMAC for space applications and maximizes the damping properties in a wide range of temperatures & frequencies Damping properties: Damping properties are ..