Polymer Property : Shear Modulus = 0.00119 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.00119 GPa
0.173 ksi
ASTM D412 Method A
Seals Eastern 5400 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.
Shear Modulus 0.00119 - 0.0115 GPa
0.173 - 1.67 ksi
Average value: 0.00466 GPa Grade Count:16
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..