Polymer Property : Shear Modulus = 0.00758 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus >= 0.00758 GPa
>= 1.10 ksi
Plate Shear, w Direction, minimum avg.
Hexcel® HexWeb® HRH-310 - 1/8 - 1.8 Aramid Fiber/Polyimide Resin Honeycomb
Designation: Material-Cell Size-DensityHexWeb HRH-310 is manufactured from aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the hexagon..