Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | >= 0.0103 GPa | >= 1.49 ksi | ASTM C273 |
Parabeam Industrie Paraglass 8 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Modulus | 0.0103 GPa | 1.49 ksi | ASTM D412 Method A |
Seals Eastern 7344 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Shear Modulus | 0.0103 GPa | 1.50 ksi | Plate Shear, W Direction, preliminary value obtained from limited testing |
Hexcel® HexWeb® HRH-78 - 3/8 - 1.5 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Shear Modulus | 0.0103 GPa | 1.50 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | 0.0103 GPa | 1.50 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/8 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |