Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Modulus = 0.0200 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus >= 0.0200 GPa
>= 2.90 ksi
ASTM C273
Parabeam Industrie ParaTank 6 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Shear Modulus 0.0200 GPa
2.90 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Modulus >= 0.0200 GPa
>= 2.90 ksi
ASTM C393
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Shear Modulus >= 0.0200 GPa
>= 2.90 ksi
ASTM C393
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Shear Modulus 0.0200 GPa
2.90 ksi
average; ASTM C393
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Copyright © lookpolymers.com All Rights Reserved