Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0240 GPa | 3.48 ksi | ASTM C273 |
SABIC Innovative Plastics ULTEM Foam XP110 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Shear Modulus | >= 0.0240 GPa | >= 3.48 ksi | ASTM C393 |
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |