Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0241 GPa | 3.50 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/4 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | 0.0241 GPa | 3.50 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/8- 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | 0.0241 GPa | 3.50 ksi | Plate Shear, W Direction, typ |
Hexcel® HexWeb® HRH-10 - 3/8 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Shear Modulus | 0.0241 GPa | 3.50 ksi | Plate Shear, W Direction, preliminary value obtained from limited testing |
Hexcel® HexWeb® HRH-78 - 3/16 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |