Mechanical Properties Metric English Comments
Shear Modulus 0.0814 GPa
11.8 ksi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP - 3/8 - 6.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..