Polymer Property : Shear Modulus = 0.309 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.309 GPa
44.8 ksi
ASTM C273
3A Composites Core Materials BALTEK® SB.150 Structural End-Grain Balsa
BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent b..