Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.410 GPa | 59.5 ksi | DIN 53457 |
Global PP-3375-RM Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-fabricsInformation provided by Global Polymers Corporation. |
|||
Shear Modulus | 0.410 GPa | 59.5 ksi | DIN 53457 |
Global PP-3370-RM Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-filmInformation provided by Global Polymers Corporation. |