Shear Modulus 0.00331 GPa
0.480 ksi
ASTM D412 Method A
Seals Eastern 7075 Ethylene-Propylene Rubber
General service EPDM.Information provided by Seals Eastern, Inc.
Shear Modulus 0.00331 GPa
0.480 ksi
Calculated; ASTM D412 Method A
Seals Eastern 7346 Extreme Low Temperature Service Rubber
HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern.