Mechanical Properties Metric English Comments
Shear Modulus 0.00428 GPa
0.621 ksi
ASTM D412 Method A
Seals Eastern 7182D Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.