Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.875 GPa | 127 ksi | calculated |
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features.. |