Polymer Property : Shear Modulus = 1.57 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.57 GPa
228 ksi
Calculated
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Shear Modulus 1.57 GPa
228 ksi
Calculated
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.