Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0700 GPa | 10.2 ksi | Typical; ASTM C273 |
Parabeam Industrie ParaTank 4.5 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Modulus | 0.0703 GPa | 10.2 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRH-10 - 1/8- 5.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |