Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | >= 0.696 GPa @Temperature -100 - 200 °C |
>= 101 ksi @Temperature -148 - 392 °F |
Average value: 2.06 GPa Grade Count:1 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |