Mechanical Properties Metric English Comments
Shear Modulus 76.3 GPa
11100 ksi
Calculated
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel
Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co..