Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 142 GPa | 20600 ksi | Calculated |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Shear Modulus | 142 GPa | 20600 ksi | Calculated |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |