Mechanical Properties Metric English Comments
Shear Modulus 146 GPa
21200 ksi
Calculated
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
DN 70 is a ZTA Alumina Toughened Zirconia.
Shear Modulus 146 GPa
21200 ksi
Calculated
CoorsTek Zirconia-Toughened Alumina, ZTA
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Shear Modulus 146 GPa
21200 ksi
Calculated
CeramTec B 40 Alumina, 99.1%
B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability.