Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 156 GPa | 22600 ksi | Calculated |
Sapco 99.7% Aluminum Oxide Information provided by Sapco. |
|||
Shear Modulus | 156 GPa | 22600 ksi | Calculated |
CoorsTek PlasmaPure-UC™ 99.9% Alumina |