Polymer Property : Shear Modulus = 165 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 165 GPa
23900 ksi
Calculated
Sapco Si.SiC Silicon Carbide
Information provided by Sapco.
Shear Modulus 165 GPa
23900 ksi
Calculated
CeramTec RK 87 Alumina, 99.8%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Shear Modulus 165 GPa
23900 ksi
Calculated
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)
Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..