Polymer Property : Shear Modulus = 189 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.30 GPa
189 ksi
calculated
BASF Capron® 1202CQ Nylon 6 (Dry)  (discontinued **)
Capron 1202CQ is a blended low viscosity, polyamide 6 injection molding homopolymer, possessing a modified crystalline structure for increased property performance and faster cycles. It is also ava..
Shear Modulus 1.30 GPa
189 ksi
in plane
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP
SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi..