Polymer Property : Shear Modulus = 2.03 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.0140 GPa
2.03 ksi
ASTM C273
SABIC Innovative Plastics ULTEM Foam XP060 PEI
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The ..
Shear Modulus >= 0.0140 GPa
>= 2.03 ksi
ASTM C393
3A Composites Core Materials AIREX® C70.48 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Shear Modulus 0.0140 - 4.73 GPa
2.03 - 685 ksi
Average value: 2.16 GPa Grade Count:10
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..