Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.43 GPa | 352 ksi | Calculated |
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Shear Modulus | 2.43 GPa | 352 ksi | Calculated |
Ascend Performance Materials VYDYNE® R400G Nylon, Mineral and Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |