Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 2.50 GPa
363 ksi
calculated
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi..
Shear Modulus 2.50 GPa
363 ksi
calculated
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined ..