Mechanical Properties Metric English Comments
Shear Modulus 1.37 - 2.60 GPa
199 - 377 ksi
Average value: 2.16 GPa Grade Count:6
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..